Zircocem
- 5 Inorganic Ceramic Adhesive Cement
|
ZIRCOCEM-5 is Zircon based Single Component Inorganic Ceramic
Adhesive Cement mainly used where high electrical insulation and
thermal conductivity are of great importance. Zireoeem-5 cures by
a chemical setting and is most ideal for potting application subject
to high temperature and high thermal shocks.
ZIRCOCEM-5
is a non corrosive and suitable inorganic adhesive cement for bonding
applications such as glass to glass, glass to ceramics, ceramics
to ceramics, ceramics to metals except Aluminum etc.
ZIRCOCEM-5
is in fine dry powder form and needs to be mixed only with clean
tap water for various cementing applications.
Characteristics |
| |
| |
Good electrical resistance |
| |
Thermal conductivity and shock
resistance |
| |
Maximum service temperature 1450°C
(2642°F) |
| |
Easy to mix and apply |
| |
Ideal for potting application
|
| |
Chemical set |
| |
Odorless |
| |
Main Uses of Zircocem-5 |
| |
i) |
Fixing /Assembly of high intensity Halogen-incandescent
lighting bulbs. |
| |
ii) |
Embedding electrical heating elements. |
| |
iii) |
Coating resistors and coils. |
| |
iv) |
Fixing thermocouples. |
| |
v) |
Mechanically sealing parts where high resistance
to electricity and thermal shock is required. |
Application Procedure
ZIRCOCEM-5
Powder should be thoroughly dry mixed before using. Weigh approximately
100 parts of powder and 10 parts clean tap water. Place powder in
a clean mixing container. Add water to the powder at one time, while
mixing do not add water gradually. continue mixing until a smooth
uniform tooth paste consistency is obtained. Mixing may be done
in slow speed mixer or by hand with a spatula. Required amount of
water should be used as per need of application, as an excess water
reduces mechanical strength, increases shrinkage and delay in setting
time. Failure of cement to adhere indicate setting has begun - discard
already mixed cement, do not attempt to retemper by adding more
water etc.
ZIRCOCEM-5 can be used by brush, trowelled, spray
by adjusting its consistency with suitable amount of water.
Setting / Curing
ZIRCOCEM-5
hardens with an internal chemical setting action after 18-24 Hrs
at ambient temp. pot life of Zircocem-5, is approximately 80 minutes
at ambient temp. when Zircocem5 powder is mixed with water. However
if desired to cure faster we suggest a gentie heat or oven drying
upto 110°C (230°F) heat should be given. Avoid steaming while drying.
Caution
To obtain
maximum bonding strength Proper curing of Zircoeem-5 is most essential.
If the cement is exposed to elevated temperature or if there is
a constant water immersion or steam environments. To avoid failures
proper drying should be done.
For high
humidity resistance, where it is impractical to heat up the cement,
a moisture resistant lacquer or Silicon coating should be applied
to the exposed surface.
Clean-up
All equipments used in preparation of adhesive cement should be thoroughly cleaned with soap and water before Zircocem-5 gets cured.
Shelf Life
ZIRCOCEM-5 Powder have safe shelf life for one year, when stored in air tight container in a dry location at ambient temperature.
Typical Properties |
| |
| |
Colour |
: Off white |
| |
Density |
: 2.56 gms/cm3 |
| |
Mixing ratio |
: Powder : 100gms
Water : 10 gms |
| |
Pot Life |
: 80 Minutes at ambient temp. |
| |
Setting time |
: 4-5 Hrs at ambient temp. depending the thickness of the cure. |
| |
Curing Time |
: 24 Hrs at ambient temp. depending upon the thickness of the cure. However
to accelerate the cure gentle heat upon 110°C (230°F). should be cTiven for 1-2 Hrs. |
NOTE : The critical range for drying cement
is between 90°C(194°F) to 110°C(230°F) Temperature should
be advanced slowly in this range to prevent rapid steam pressure
which can cause spalling and disruption of the cement.
| |
Linear shrinkage |
: 0.4 - 0.6% |
| |
Co-efficient of thermal expansion (25°C - 1000°C) |
: 4.32 x 10-6 / °C |
| |
Compressive Strength |
: 230Kg/cm2 |
| |
Dielectric constant |
: 6.8 |
| |
Volume Resistivity (at 25°C) |
: 1.45 x 1011 ohm-cm |
| |
Dielectric Strength |
: 2165 Volts/mm |
| |
Tensile Strength |
: 46 Kg/cm2 (654PSI) |
| |
Max.Service Temp. |
: 1450°C |
|